Non Woven Fabric Manufacturing Machine: Spunbond vs. Meltblown and How to Choose the Right Technolog

Non woven fabric applications

Spunbond Technology: The Foundation of Strength

A spunbond non woven fabric manufacturing machine transforms polymer granules into continuous filaments through a multi-stage process:

  1. Polymer melting and extrusion through a spinneret
  2. Filament attenuation using high-velocity cool air
  3. Web formation on a conveyor
  4. Thermal or mechanical bonding for stability

Corrected / Verified Technical Points

  • Spunbond fibers are continuous and typically 15–40 microns in diameter.
  • Fiber orientation during drawing increases tensile strength, which is why spunbond fabrics are used where durability matters.
  • Bonding is usually done by hot calender rollers, not chemical bonding (chemical bonding exists in the industry but is uncommon in spunbond lines).

Key Advantages

  • High tensile strength and tear resistance
  • Good breathability
  • High production output and lower cost per kg

Primary Applications

  • Hygiene products (diapers, wipes, sanitary covers)
  • Medical gowns (outer and inner layers)
  • Geotextiles and roofing membranes
  • Agricultural crop covers and packaging materials
Non woven fabric applications

Meltblown Technology: The Filtration Expert

  1. Polymer is extruded through extremely small die orifices
  2. High-temperature compressed air attenuates the melt into microfibers
  3. Fibers self-bond while landing on the collector

Corrected / Verified Technical Points

  • Meltblown fibers range from 1–5 microns, sometimes below 1 micron with advanced dies.
  • The web forms primarily through fiber entanglement, not secondary thermal calendering.
  • Meltblown fabrics are intrinsically weaker because fibers are discontinuous.

Key Advantages

  • Exceptional filtration efficiency
  • High surface area ideal for absorption
  • Superior barrier properties

Primary Applications

  • Medical mask filtration layers (N95 / surgical)
  • HEPA/ULPA air filters
  • Oil absorption materials
  • Liquid filtration
Non Woven Fabric Primary Applications

Core Technical Differences Between the Two Machines

Feature / MechanismSpunbond MachineMeltblown Machine
Fiber TypeContinuous filamentsDiscontinuous microfibers
Fiber Diameter15–40 µm1–5 µm
Air SystemCold air for drawingHot, high-pressure air for fiber splitting
BondingThermal calenderingMostly self-bonding
StrengthHighLow
Filtration PerformanceLowVery high

Performance Comparison: Strength vs. Protection

  • Spunbond: Think of it as the muscle—strong, durable, and ideal for structural layers.
  • Meltblown: Think of it as the shield—excellent at trapping particles and fluids, but mechanically weaker.

This is why many manufacturers choose SMS composite machines (Spunbond–Meltblown–Spunbond) to combine both benefits.

Investment, Energy Use, and Market Reality

Initial Investment

  • Spunbond machines: Higher cost, larger footprint
  • Meltblown machines: Smaller footprint, generally lower capital requirement

Operational Costs

  • Meltblown machines consume more energy due to high-temperature compressed air
  • Spunbond machines offer better energy efficiency per kilogram

Market Stability

  • Meltblown demand fluctuates (spikes during health emergencies)
  • Spunbond demand remains steady across hygiene, agriculture, construction, and packaging

Choose Spunbond if you need to produce:

  • Large-volume, durable fabrics
  • Agricultural covers, hygiene layers, geotextiles, packaging

Choose Meltblown if you target:

  • High-value filtration markets
  • Medical masks, air filters, sorbents, insulation

Choose SMS Composite Lines if you want:

  • Maximum production flexibility
  • Ability to enter multiple industries with one system

Related Recommendations

Scroll to Top

Contact us now